FED-STD-791D
100 (A + B)
Percent insolubles =
W
where:
A = increase in weight of Gooch crucible.
B = increase in weight of centrifuge tube.
W = original weight of oil sample.
8. REPORTING
8.1 Report the following:
weight change of the metal strip before brushing.
a.
b.
weight change of the metal strip after brushing.
change in acid number of the sample.
c.
d.
acid number of the water layer after hydrolysis.
e.
change in viscosity of the oil.
f.
weight of insolubles formed during hydrolysis.
g.
color of the oil after hydrolysis.
h.
general appearance of the sample after hydrolysis.
9. PRECISION
9.1 Precision data have not been developed for this method.
Method Prepared By: